品名镍基合金粉 产地河北邢台镍含量≥85(%)粒度80-150 150-300(目)牌号fnin-25a包装规格桶形状球形制作方法雾化法 凡金属合金粉 末都可以用于等离子喷涂,氧乙炔火焰喷涂以及超音速喷涂,以下介绍是我公司生产的常用的典型喷涂粉 末,建议用户在使用前必须在炉内加热到120℃保温两小时后,随炉冷至常温即可使用。
all of the metal alloy powders can be used for plasma spraying, oxyacetylene flame spraying【敏感词】supersonic spraying, the following typical sprayed coating powder should be heated in the stove until 120℃. then, the heat of the power should be preserved for two hours【敏感词】later be cooled to the normal temperature before useing.